February 02, 2026 article Open access Data-driven artificial intelligence methods for real-time welding defect diagnosis: A critical review and future outlook Journal of Manufacturing Processes DOI: 10.1016/j.jmapro.2026.01.101 Full text (OA) OpenAlex Authors 0 Author list not loaded yet. Cited by 0 stored of 7 References 1 Search Sort Most cited Newest Oldest Patent citations Title Any typearticle review book-chapter conference-paper preprint dissertation book dataset other Any fieldAgricultural and Biological Sciences Arts and Humanities Biochemistry, Genetics and Molecular Biology Business, Management and Accounting Chemical Engineering Chemistry Computer Science Decision Sciences Dentistry Earth and Planetary Sciences Economics, Econometrics and Finance Energy Engineering Environmental Science Health Professions Immunology and Microbiology Materials Science Mathematics Medicine Neuroscience Nursing Pharmacology, Toxicology and Pharmaceutics Physics and Astronomy Psychology Social Sciences Veterinary Open access A Spatio-Temporal Ensemble Deep Learning Architecture for Real-Time Defect Detection during Laser Welding on Low Power Embedded Computing Boards 2021 Sensors article Engineering Industrial Vision Systems and Defect Detection Open access cited by 1 patent 71 citations 1 result