Atomic layer deposition for efficient oxygen evolution reaction at Pt/Ir catalyst layers
Beilstein Journal of Nanotechnology, vol. 11, pp. 952–959
Abstract
We provide a direct comparison of two distinct methods of Ti felt surface treatment and Pt/Ir electrocatalyst deposition for the positive electrode of regenerative fuel cells and vanadium–air redox flow batteries. Each method is well documented in the literature, and this paper provides a direct comparison under identical experimental conditions of electrochemical measurements and in identical units. In the first method, based on classical engineering, the bimetallic catalyst is deposited by dip-coating in a precursor solution of the salts followed by their thermal decomposition. In the alternative method, more academic in nature, atomic layer deposition (ALD) is applied to the felts after anodization. ALD allows for a controlled coating with ultralow noble-metal loadings in narrow pores. In acidic electrolyte, the ALD approach yields improved mass activity (557 A·g−1 as compared to 80 A·g−1 at 0.39 V overpotential) on the basis of the noble-metal loading, as well as improved stability.
Authors 7
-
Friedrich-Alexander-Universität Erlangen-Nürnberg
Affiliation as printed
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany,
-
DWI – Leibniz Institute for Interactive Materials
Affiliation as printed
DWI-Leibniz Institute for Interactive Materials, Forckenbeckstr. 50, 52074 Aachen, Germany
DWI-Leibniz Institute for Interactive Materials, Forckenbeckstr. 50, 52074 Aachen, Germany,
-
Stefanie M. A. Kriescher Aachen
Affiliation as printed
RWTH Aachen University Aachener Verfahrenstechnik-Chemical Process Engineering, Forckenbeckstr. 51, 52074 Aachen, Germany
RWTH Aachen University Aachener Verfahrenstechnik-Chemical Process Engineering, Forckenbeckstr. 51, 52074 Aachen, Germany,
-
Friedrich-Alexander-Universität Erlangen-Nürnberg
Affiliation as printed
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany,
-
Society for Chemical Engineering and Biotechnology · DECHEMA-Forschungsinstitut
Affiliation as printed
DECHEMA-Forschungsinstitut, Theodor-Heuss-Allee 25, 60486 Frankfurt am Main, Germany
DECHEMA-Forschungsinstitut, Theodor-Heuss-Allee 25, 60486 Frankfurt am Main, Germany and
-
DWI – Leibniz Institute for Interactive Materials
Affiliation as printed
DWI-Leibniz Institute for Interactive Materials, Forckenbeckstr. 50, 52074 Aachen, Germany
DWI-Leibniz Institute for Interactive Materials, Forckenbeckstr. 50, 52074 Aachen, Germany,
-
Julien Bachmann corresponding
St Petersburg University · Friedrich-Alexander-Universität Erlangen-Nürnberg
Affiliation as printed
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany
Saint Petersburg State University, Institute of Chemistry, Universitetskii pr. 26, 198504 St. Petersburg, Russia
Friedrich-Alexander-Universität Erlangen-Nürnberg, Chair 'Chemistry of Thin Film Materials', IZNF, Cauerstr. 3, 91058 Erlangen, Germany,
Cited by 11 stored of 11
11 results
No patents citing this paper on Lens.org (checked 2026-10-06).
References 28
-
W1993256145details pending0citations